ExxonMobil Exxtral™ CNU 015 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ CNU 015 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessGood Impact ResistanceGood Surface FinishLow EmissionsLow to No FoggingNon-sticky Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527-2/50
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527-2/50
Elongation at Break 70 %
70 %
ISO 527-2/50
Elongation at Yield 5.0 %
5.0 %
ISO 527-2/50
Tensile Modulus 1.45 GPa
210 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.651 J/cm²

@Temperature 0.000 °C
3.10 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
1.05 J/cm²

@Temperature 22.8 °C
5.00 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ISO 75-2/A