ExxonMobil Exxtral™ H1725W Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ H1725W Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with very high flow. Product presenting very high rigidity, maintaining excellent impact resistance properties, including at a low temperature. UV stabilized version.Availability: Europe Features:Balanced Stiffness/ToughnessGood UV Resistance High FlowHigh Impact ResistanceLow Temperature Impact Resistance Uses: Automotive ApplicationsAutomotive Exterior PartsAutomotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-2/50
Flexural Modulus 1.60 GPa
232 ksi
ISO 178
Charpy Impact, Notched 0.798 J/cm²

@Temperature -30.0 °C
3.80 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
6.09 J/cm²

@Temperature 22.8 °C
29.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A