Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with very high stiffness, high heat ageing resistance and detergent resistance designed for electrical applications such as washing machines.Availability: Europe Features:Good Dimensional StabilityGood Surface FinishLow WarpageUltra High StiffnessUses: Appliance ComponentsAppliancesProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 MPa
4210 psi
ISO 527-2/50
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2/50
Elongation at Break 5.0 %
5.0 %
ISO 527-2/50
Elongation at Yield 3.2 %
3.2 %
ISO 527-2/50
Tensile Modulus 4.25 GPa
616 ksi
Secant; ISO 527-2
Flexural Modulus 4.35 GPa
631 ksi
ISO 178
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
ISO 75-2/A