Material Notes:
Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable production of products free of taste and odor for food and beverage packaging.Availability: Latin America, North America and South America Additive: Antioxidant: YesApplications: Food Packaging ContainersFood Service TraysHouseware ArticlesHousewares Toys Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Melt Flow 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.44 MPa
3400 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 0.9653 GPa
140.0 ksi
2% Secant; ASTM D790
Izod Impact, Notched 0.224 J/cm

@Temperature -40.0 °C
0.420 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
Descriptive Properties Value Comments
Features Standard Processing Antioxidants Stabilizer
Form Pellet