Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. Ideally suited for articles requiring low warpage, glossy surfaces and cold temperature impact resistance.Availability: Latin America, North America and South America Additive: Antioxidant: YesApplications: Food Packaging ContainersHouseware ArticlesLawn & Garden AccessoriesSoda Carrier TotesToysInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ExxonMobil method
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.86 MPa
270 psi
ASTM D638
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
2% Secant; ASTM D790B
Flexural Modulus, 1% Secant 1240 MPa
180000 psi
ASTM D790B
Izod Impact, Notched 0.326 J/cm

@Temperature -40.0 °C
0.610 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 267 °C
<= 513 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 73.3 °C
164 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 45.6 °C
114 °F
ASTM D648B
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved