ExxonMobil HDPE HTA 002 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HTA 002 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can also be used pure, especially for easy processing and conversion into small and thin bags, to be used for light item packaging. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications: Blown FilmCollation ShrinkFood packagingGeneral PackagingGrocery SacksHeavy Duty BagsIndustrial PackagingLabel FilmShrink FilmStand Up PouchesThin Gauged Consumer Bags Trash BagsTrash Can LinersInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 16 g/10 min

@Load 21.6 kg,
Temperature 190 °C
16 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 29.0 MPa
4200 psi
ASTM D882
Film Tensile Strength at Yield, TD 29.0 MPa
4200 psi
ASTM D882
Film Elongation at Break, MD 320 %
320 %
ASTM D882
Film Elongation at Break, TD 450 %
450 %
ASTM D882
Elmendorf Tear Strength MD 8.0 g
8.0 g
ASTM D1922
Elmendorf Tear Strength TD 60 g
60 g
ASTM D1922
Dart Drop Test 160 g
0.353 lb
ASTM D1709A
Film Tensile Strength at Break, MD 55.2 MPa
8000 psi
ASTM D882
Film Tensile Strength at Break, TD 50.3 MPa
7300 psi
ASTM D882
1% Secant Modulus, MD 965 MPa
140000 psi
ASTM D882
1% Secant Modulus, TD 1170 MPa
170000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525