ExxonMobil Isopar™ L (AM) Isoparaffin Fluid

Category Fluid
Manufacturer Exxon Chemical
Trade Name Isopar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Isopar™ L (AM) Isoparaffin Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Central America, South America and North AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.405 g/cc

@Temperature 15.6 °C
0.0146 lb/in³

@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 2.02 cSt
2.02 cSt
ASTM D445
Vapor Pressure 0.000400 bar

@Temperature 20.0 °C
0.300 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 189 °C
372 °F
Initial; ASTM D86
Flash Point 62.2 °C
144 °F
ASTM D56
Descriptive Properties Value Comments
Aniline Point 185°F
Method E, ASTM D611
Aromatic Content 20 wt ppm
UV, ExxonMobil Method
Dry Point 408°F
ASTM D86