Material Notes:
Appearance: Clear, free of suspended matterAvailability: North AmericaCAS Number: 64742-53-6Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.860 - 0.900 g/cc
0.0311 - 0.0325 lb/in³
BRCP 4843
Maximum Moisture Content 0.10
0.10
BRCP 5053
Descriptive Properties Value Comments
Color <250
Platinum Cobalt, BRCP 4273