Material Notes:
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength properties, along with excellent drawability of these resins, make them versatile packaging film resins.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: No Thermal Stabilizer: YesApplications: Cast FilmCast Stretch FilmPackaging Films Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.9180 g/cc
0.03316 lb/in³
ExxonMobil Method
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
Film Tensile Strength at Yield, TD 6.76 MPa
980 psi
ASTM D882
Film Elongation at Break, MD 560 %
560 %
ASTM D882
Film Elongation at Break, TD 830 %
830 %
ASTM D882
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
Elmendorf Tear Strength, MD 9.84 g/micron
250 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 22.4 g/micron
570 g/mil
ASTM D1922
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 58.6 MPa
8500 psi
ASTM D882
Film Tensile Strength at Break, TD 36.5 MPa
5300 psi
ASTM D882
1% Secant Modulus, MD 117 MPa
17000 psi
ASTM D882
1% Secant Modulus, TD 124 MPa
18000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 123 °C
254 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.7 %
1.7 %
ASTM D1003
Gloss 90 %
90 %
45°; ASTM D2457
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: