Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications that require excellent processability and ESCR along with the optimum balance of stiffness and low temperature toughness. Availability: Latin America, North America and South America Additive: Stabilizer: YesLong Term UV-15 Applications: Agricultural Tank LinersConsumer ArticlesExternally supported intermediate bulk containersLarge Sized Industrial PartsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ExxonMobil method
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693B
ESCR 10% Igepal® 650 hour
650 hour
ASTM D1693B
Melt Flow 5.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.2 MPa
2200 psi
2.0 in/min; ASTM D638
Elongation at Yield 20 %
20 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 600 MPa
87000 psi
ASTM D638
Impact Test 88.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
65.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point <= 259 °C
<= 498 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 36.7 °C
98.0 °F
ASTM D648