Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high energy layer and can be printed with water-based or solvent-based flexo and gravure inks and UV cured inks.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Coating Weight >= 11.4 g/m²
>= 7.10 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
510
Film Elongation at Break, TD 45 %
45 %
510
Coefficient of Friction 0.32
0.32
430
Film Tensile Strength at Break, MD 138 MPa
20000 psi
510
Film Tensile Strength at Break, TD 262 MPa
38000 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 6.0 %
6.0 %
at 275°F; 438
Shrinkage, TD 6.0 %
6.0 %
at 275°F; 438
Optical Properties Metric English Comments
Haze 1.4 %
1.4 %
444
Gloss 93 %
93 %
442
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Wetting Tension, receding COS theta 0.8
machinable
0.85
high energy surface
Yield, in2/lb 61200
Users viewing this material also viewed the following: