Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured inks. It is designed to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers, such as Krones Topmatic labeling equipment. Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 91.4 microns
3.60 mil
Coating Weight >= 43.7 g/m²
>= 27.3 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 86 %
86 %
510
Film Elongation at Break, TD 25 %
25 %
510
Film Tensile Strength at Break, MD 42.13 MPa
6111 psi
510
Film Tensile Strength at Break, TD 80.441 MPa
11667 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %
3.0 %
at 275°F; 438
Shrinkage, TD 3.0 %
3.0 %
at 275°F; 438
Optical Properties Metric English Comments
Transmission, Visible 18 %
18 %
417
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 18
Gurley Stiffness, TD, mgf 30
Yield, in2/lb 15800