ExxonMobil Label-Lyte® ROSO 50 LR-210 Clear OPP Shrink Film

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® ROSO 50 LR-210 Clear OPP Shrink Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear, machine-directions shrinkable, polypropylene film. Designed for use as a monoweb in roll-fed labeling of contoured containers such as aluminum and steel beverage cans, beaded metal cans, aerosol containers, and contoured glass and plastic bottles. The treated clear layer is intended to be reverse-printed with solvent-based or water-based flexo and gravure inks and UV-cured inks.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Coating Weight >= 44.6 g/m²
>= 27.9 lb/ream
520
Thermal Properties Metric English Comments
Shrinkage, MD 19 %
19 %
at 275°F; 438
Shrinkage, TD 2.0 %
2.0 %
at 275°F; 438
Optical Properties Metric English Comments
Haze 2.8 %
2.8 %
444
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Wetting Tension 40
dyne/cm
Yield, in2/lb 15000