Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Mytex™ AS65KW-1ATM

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name Mytex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mytex™ AS65KW-1ATM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84
84
Tensile Strength, Yield 24.0 MPa
3480 psi
2 in/min; LAB032
Flexural Modulus 2.400 GPa
348.1 ksi
1% tangent, 0.05 in/min.; LAB033
Izod Impact, Notched 4.00 J/cm
7.50 ft-lb/in
LAB034
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
LAB036
Users viewing this material also viewed the following: