Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate

Category Polymer , Adhesive , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Molding Grade
Manufacturer Exxon Chemical
Trade Name OPTEMA™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low as 200°F and up to 600°F.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesApplications: CompatibilizerEngineering Polymer ToughenerLow Temperature Sealant CompoundsMasterbatch Base ResinInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ExxonMobil Method
Methyl Acrylate Content 24 %
24 %
Melt Flow 5.00 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
15s; ASTM D2240
Hardness, Shore D 24
24
15s; ASTM D2240
Tensile Strength at Break 5.86 MPa
850 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0248 GPa
3.60 ksi
1% secant; ASTM D790
Impact Test 14.9 J

@Temperature 23.0 °C
11.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
20.3 J

@Temperature -40.0 °C
15.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 45.0 °C
113 °F
ASTM D1525