Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Compounding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where softness and flexibility are required.Applications: Coextruded tie layer for flexible packaging applications; Compatibilizer or impact modifier for engineering thermoplastics; Hot melt adhesives; Sealants.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
Exxon Method
Melt Flow 5.0 g/10 min
5.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
ASTM D2240
Hardness, Shore D 28
28
ASTM D2240
Tensile Strength, Ultimate 8.00 MPa
1160 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0190 GPa
2.76 ksi
ASTM D790
Tensile Impact Strength 590 kJ/m²
281 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 64.0 °C
147 °F
Exxon Method
Vicat Softening Point 39.0 °C
102 °F
1000g; ASTM D-1525