Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP1105E1 Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP1105E1 Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: High melt flow rate homopolymer. Particularly suitable for general purpose injection molding.Availability: North America Features:Controlled RheologyGeneral PurposeGood ProcessabilityHigh FlowNarrow Molecular WeightUses: Automotive ApplicationsConsumer ApplicationsFabricsFibersNonwovesnPackagingProcessing Method: Compounding and Injection Blow MoldingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.4 MPa
5130 psi
2 in/min; ASTM D638
Elongation at Yield 23 %
23 %
ExxonMobil Method
Flexural Modulus 1.47 GPa
213 ksi
1% secant, 0.05 in/min.; ASTM D790A
Izod Impact, Notched 0.294 J/cm
0.550 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Users viewing this material also viewed the following: