Material Notes:
Medium melt flow rate homopolymer, 20% filled. Particularly suitable for consumer products and appliance applications requiring long term heat aging resistance. UL continuous service rating of 95°C.Availability: North America Features:Detergent ResistantFilledGood Thermal Ageing ResistanceHigh Heat ResistanceHigh StiffnessMedium Flow Automotive Specifications: CHRYSLER MS-DB500Processing Method: Extrusion and Injection MoldingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.8 MPa
5340 psi
2 in/min; ASTM D638
Elongation at Yield 5.8 %
5.8 %
2 in/min; ASTM D638
Flexural Modulus 0.239 GPa
34.7 ksi
1% secant, 0.05 in/min.; ASTM D790A
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
253 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 215 - 260 °C
419 - 500 °F
Copyright © lookpolymers.com All Rights Reserved