Material Notes:
Product Description: A clarified homopolymer resin designed for production of extruded sheet and thermoformed containers. It exhibits excellent processing characteristics even in deep drawn applications.Availability: North America Features:Autoclave SterilizableEthylene Oxide SterilizableLow EmissionsSteam SterilizableUses: CupsPackagingRigid PackagingProcessing Method: Blow Molding, Extrusion, Extrusion Blow Molding, Injection Blow Molding, Profile Extrusion, Sheet Extrusion and ThermoformingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.8 MPa
5340 psi
2.0 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1710 MPa
248000 psi
0.05 in/min; ASTM D790A
1940 MPa
281000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.497 J/cm
0.930 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003