Material Notes:
Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good ColorabilityGood Dimensional StabilityGood Thermal StabilityMedium FlowUses: Automotive ApplicationsCapsClosuresCompoundingPackagingRigid PackagingProcessing Method: Injection MoldingAutomotive Certifications: Chrysler MS DB500 CPN 2194Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.9 MPa
3460 psi
2 in/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
2 in/min; ASTM D638
Flexural Modulus 1.08 GPa
157 ksi
1% secant, 0.05 in/min.; ASTM D790A
1.25 GPa
181 ksi
1% secant, 0.5 in/min; ASTM D790B
Izod Impact, Notched NB
NB
ASTM D256
Gardner Impact 28.2 J

@Thickness 3.17 mm,
Temperature -30.0 °C
20.8 ft-lb

@Thickness 0.125 in,
Temperature -22.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 204 - 246 °C
399 - 475 °F
Typical