ExxonMobil PP9513 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP9513 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A random copolymer resin designed for non-oriented film.Availability: North America Features:Controlled RheologyEthylene Oxide SterilizableUses: BagsCast FilmHeavy-duty BagsPackagingProcessing Method: Cast FilmInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.6 MPa
3720 psi
2.0 in/min; ASTM D638
Elongation at Yield 13 %
13 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 896 MPa
130000 psi
0.05 in/min; ASTM D790A
1050 MPa
153000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.513 J/cm
0.960 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648