Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Key Features:Recommended for applications requiring excellent flex fatigue resistance.Excellent ozone resistance.Designed for improved UV resistance.Designed for extruding thin sections with excellent definition (down to 0.33 mm [0.013"] radius). Long runs with minimal build-up of material on screen packs or narrow die sections.EU and China RoHS compliant.Applications:Automotive- Weather SealsUses:Automotive ApplicationsAutomotive Interior Trim Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemcial
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
2 mm, 15 sec; ISO 868
67
67
Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 4.50 MPa
653 psi
Air at 302°F, 168 hr; ASTM D573
5.00 MPa
725 psi
Across Flow; ASTM D412
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 440 %
440 %
Across Flow; ASTM D412
475.2 %
475.2 %
Air at 302°F, 168 hr; ASTM D573
Tear Strength 36.1 kN/m
206 pli
73°F, Die C; ASTM D624
Compression Set 18 %
18 %
73°F, 22 hr; ASTM D395
39 %
39 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.7
2.7
1.96 mm; ASTM D150
Dielectric Strength 25.6 kV/mm
650 kV/in
2.03 mm; ASTM D149
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Die Temperature 204 °C
400 °F
Extrusion
Melt Temperature 177 - 204 °C
350 - 400 °F
Extrusion
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Back Pressure 5.00 - 20.0 MPa
725 - 2900 psi
Extrusion
Descriptive Properties Value Comments
Color Black
Form Pellets
Users viewing this material also viewed the following: