Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8211-65M300 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good appearance. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Excellent ozone resistance.Used in sealing applications.Recommended for applications requiring excellent flex fatigue resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55

@Thickness 2.00 mm
55

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 4.69 MPa
680 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.07 MPa
300 psi
Across Flow; ASTM D412
Elongation at Break 420 %
420 %
Across Flow; ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets