Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Film Grade
Manufacturer Exxon Chemical
Trade Name Vistamaxx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistamaxx™ 3020FL Propylene-based Elastomer - High Purity, Low Gel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Vistamaxx 3020FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. The "FL" designates this is a high purity grade with very low gel content, making it suitable for premium and performance film and molding applications.Key Features:Suitable for a wide range of blown film and molding applications where improved melt strength is desired.Can be blended with PP, PE and other polyolefins.Excellent toughness in terms of tear and puncture resistance with good processability for stretch hood cores.Good optical properties.Good sealing properties.Good organoleptic properties.Good chemical resistance to aqueous systems and non-hydrocarbon based fluids.May be used in food contact applications (with some restrictions).EU and China RoHS compliant.Applications:Blown FilmPolymer ModificationCompoundingThermoformingUses:CompoundingFilmPackaging Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.874 g/cc
0.874 g/cc
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
melt flow rate; ExxonMobil Method
1.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore D 34

@Time 15.0 sec
34

@Time 0.00417 hour
ASTM D2240
Tensile Stress 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ASTM D412
4.40 MPa

@Strain 300 %
638 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 4.70 MPa
682 psi
ASTM D412
Elongation at Yield 47 %
47 %
ASTM D412
Flexural Modulus, 1% Secant 60.0 MPa
8700 psi
ASTM D790
Tear Strength 64.3 kN/m
367 pli
Die C; ASTM D624
Tensile Set 49 %
49 %
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
ASTM D1525
Descriptive Properties Value Comments
Ethylene Content 10.5 wt%
ASTM D3900