Material Notes:
Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, is easy to process and is compatible with a wide variety of materials. It is particularly good for thermoplastic and polyolefinic blends where a balance of flexibility, transparency and impact performance is required.Key Features:Suitable for a wide range of blown and cast film applications, extrusion coating and lamination applications.Other typical applications include calendered or extruded sheet/profiles, injection molded goods and nonwovens.Excellent adhesion to conventional or metallocene PP and PE.Very good elasticity and toughness.Very low seal initiation temperature combined with high seal strength when used as sealing layer of co-extruded structures.Very good chemical resistance and long term aging.Particularly good for thermoplastic and polyolefinic blends where a balance of flexibility, transparency and impact performance is required.EU and China RoHS compliant.Applications:Calendered ProfilesExtrueded profilesPP/TPE ModificationCalendered SheetingExtruded SheetingCast FilmInjection Molding Uses:CompoundingFilmPackaging Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.863 g/cc
0.863 g/cc
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
melt flow rate; ExxonMobil Method
9.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ASTM D2240
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ASTM D412
Flexural Modulus, 1% Secant 12.3 MPa
1780 psi
ASTM D790
Tear Strength 33.0 kN/m
188 pli
Die C; ASTM D624
Tensile Set 18 %
18 %
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 47.1 °C
117 °F
ASTM D1525
Descriptive Properties Value Comments
Ethylene Content 15.0 wt%
ASTM D3900
Copyright © lookpolymers.com All Rights Reserved