Fainplast Compounds CKL 0252/R Flexible PVC, Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds CKL 0252/R Flexible PVC, Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral oil resistant sheathing
Physical Properties Metric English Comments
Density 1.27 - 1.31 g/cc
0.0459 - 0.0473 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77
73 - 77
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 330 %
>= 330 %
ISO R 527
Descriptive Properties Value Comments
Thermal Stability (minutes) 55
CEI 20-34/3-2