Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Fainplast Compounds
Trade Name Ethylplus
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 0.933 g/cc
0.0337 lb/in³
ISO 1183
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
ISO 868
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
50 mm/min; ISO 527
Elongation at Break >= 300 %
>= 300 %
50 mm/min; ISO 527
Electrical Properties Metric English Comments
Volume Resistivity >= 5.00e+15 ohm-cm
>= 5.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 180 - 240 °C
356 - 464 °F
Users viewing this material also viewed the following: