Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds GS 100/2 Flexible PVC, Injection Molding, Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GS 100/2 Flexible PVC, Injection Molding, Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-rigid for cable passage
Physical Properties Metric English Comments
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 67 - 71
67 - 71
± 2; ISO R 868
Tensile Strength at Break 20.0 MPa
2900 psi
ISO R 527
Elongation at Break 150 %
150 %
ISO R 527
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved