Fainplast Compounds HAX HF 28 Halogen Free PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name HAX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HAX HF 28 Halogen Free PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheathing; good mechanical properties
Physical Properties Metric English Comments
Density 1.46 - 1.50 g/cc
0.0527 - 0.0542 lb/in³
IEC 60811
Melt Index of Compound 4.0 g/10 min

@Load 21.6 kg,
Temperature 150 °C
4.0 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 47 - 53
47 - 53
IEC 60811
Tensile Strength at Break 13.0 MPa
1890 psi
IEC 60811
Elongation at Break 190 %
190 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 35 %
35 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm

@Temperature 20.0 °C
3.00e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257