Fainplast Compounds KL 95 Flexible PVC, Insulation for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds KL 95 Flexible PVC, Insulation for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive cables low thickness
Physical Properties Metric English Comments
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 95
91 - 95
ISO R 868
Elongation at Break >= 240 %
>= 240 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+13 ohm-cm

@Temperature 23.0 °C
8.00e+13 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 220
CEI 20-34/3-2