Fainplast Compounds PK 8350 Flexible PVC, Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PK 8350 Flexible PVC, Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheath according to normal fiat type 70 9.91220 All. 28
Physical Properties Metric English Comments
Density 1.40 - 1.44 g/cc
0.0506 - 0.0520 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 86
82 - 86
ISO R 868
Tensile Strength at Break 12.0 MPa
1740 psi
ISO R 527
Elongation at Break 250 %
250 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
Cold Flex; ISO 458/2