Fibre Glast 180 Clear Gel Coat

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 180 Clear Gel Coat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
#180 Clear Gel Coat is a high performance, premium quality gel coat for both airless and air atomized spray applications. #180 offers UV light stability, excellent clarity, crack and chemical resistance. This deep, crystal-clear and non-yellowing gel coat is compatible with underwater and water contact marine applications as well as sanitary ware such as showers and tubs. It is recommended to be used as a protective clear coat over Chromaveilâ„¢, other colors or glitterflake. Blend with #1040 Duratec Hi-Gloss Additive when top coating. Requires 1.5% MEKP
Physical Properties Metric English Comments
Viscosity 10000 - 13000 cP

@Shear Rate 0.100 1/s,
Temperature 25.0 °C
10000 - 13000 cP

@Shear Rate 0.100 1/s,
Temperature 77.0 °F
LVF#4, Uncured
17000 - 22000 cP

@Shear Rate 1.00 1/s,
Temperature 25.0 °C
17000 - 22000 cP

@Shear Rate 1.00 1/s,
Temperature 77.0 °F
LVF#4, Uncured
Viscosity Measurement 5.9 - 6.5
5.9 - 6.5
Thix Index, Uncured
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Gel Time 8.00 - 10.0 min
8.00 - 10.0 min
Descriptive Properties Value Comments
Peak Cure Exotherm 390-405°F