Fibre Glast 182 White Gel Coat

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 182 White Gel Coat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
#182 White Gel Coat is a highly durable ISO gel coat and is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spray un-thinned into molds using a cup gun or blend with #1040 Duratec Hi-Gloss Additive when performing repairs. Approved for use in marine and sanitary ware applications. Requires 1.5% MEKPFeatures & Benefits: Shelf Stability; Ease of application; Flexural strength; Crack resistance; Chemical Resistance; Tear Resistance; Long term durability; UV Light Stability; Water/osmosis resistance
Physical Properties Metric English Comments
Density 1.08 - 1.38 g/cc
0.0390 - 0.0498 lb/in³
Viscosity 2300 - 2900 cP

@Shear Rate 1.00 1/s,
Temperature 25.0 °C
2300 - 2900 cP

@Shear Rate 1.00 1/s,
Temperature 77.0 °F
LVF#4, Uncured
Viscosity Measurement 4.5 - 6.5
4.5 - 6.5
Thix Index, Uncured
Mechanical Properties Metric English Comments
Elongation at Break 1.7 - 2.2 %
1.7 - 2.2 %
Flex; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 - 98.9 °C
180 - 210 °F
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
40 - 60 minute film cure
Gel Time 8.00 - 12.0 min

@Temperature 25.0 °C
8.00 - 12.0 min

@Temperature 77.0 °F