Fibre Glast 2443 Kevlar® Twill Weave Fabric

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 2443 Kevlar® Twill Weave Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Kevlar® fabric provides the improved cosmetics and drapability of a twill weave. Ideal for impact resistant applications requiring the lightweight, high strength properties of Kevlar® where pattern show-through is desirable.
Descriptive Properties Value Comments
Weave Pattern 2x2 twill
Weight (oz/sq yd) 5.3
Yarn Description, Fill 1140 Denier Kevlar® 49
Yarn Description, Warp 1140 Denier Kevlar® 49