Material Notes:
#71 Styrene Wax is a 5% solution of paraffin dissolved in styrene that may be added to non waxed polyester resins and gel coats to prevent the prolonged tackiness associated with thin sections of polyesters. If the resin contains paraffins, the wax will rise to the surface and protect the curing resin from the inhibiting action of the air. However, if the resin is allowed to fully cure, the paraffins on the surface will prevent adhesion of further coats of resin and must be sanded off prior to additional applications. Fibre Glast recommends adding #71 at 5% for thin coatings. Use with #1040 Hi-Gloss Additive when performing repairs below the water line.
Physical Properties Metric English Comments
Specific Gravity 0.910 - 0.911 g/cc

@Temperature 15.6 °C
0.910 - 0.911 g/cc

@Temperature 60.0 °F
ASTM D891
Descriptive Properties Value Comments
Aldehyde (wt. %) <0.02
ASTM D2119-87
Benzene (ppm) <0.0001
ASTM D5135
Color (Pt. Co.) 10 (Typical)
ASTM D5386
Ethylbenzene (ppm) <0.008
ASTM D5135
Inhibitor 0.001 - 0.0015
ASTM D4590
Peroxides (wt. %) <0.01
ASTM D2340-82
Polymer (ppm) <0.001
ASTM D2121-90
Styrene >99.7
ASTM D5135
Total Chlorides (wt. %) <0.0001
ASTM D4929
Total Sulfur (wt. %) <0.0001
ASTM D3246
Copyright © lookpolymers.com All Rights Reserved