Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 permits fast wet-out in spray or hand laminates. Its 225°F service temperature also resists exotherm and post cure problems. Properly fabricated parts may be used in food service applications. #90 is a pre-promoted, thixotropic, corrosion and temperature-resistant Isophthalic polyester resin. This versatile product features a high molecular weight and crosslink density and offers good corrosion resistance in a variety of aqueous and acidic media. The performance of #90 has been proven by over 30 years of successful service.Features:High molecular weight Isophthalic polymerContains no esterification catalystChemical components listed under FDA 177.2420 Title 21Laminates based on #90 can meet BS 6920 requirementsLaminates can meet MIL-R-7575C Grade A and B with Class 0 and 3 Electrical PropertiesManufactured using statistical controls in ISO-9002 certified plantsBenefits:Corrosion resistance, Strength, ToughnessSuperior corrosion and blister resistanceCan be used in food and beverage contact applicationApproved for use in military applicationsConsistent batch to batch performanceProperties are listed for 1/8" Laminate, 4 plies of 1.5 oz/ft2 chopped strand mat. Glass content: 35% by weight: Thickness 0.090", at Room Temperature of 77°FInformation provided by Fibre Glast Developments Corporation.
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Tensile Strength at Break 123 MPa
17900 psi
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 216 MPa
31400 psi
ASTM D790
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Compressive Yield Strength 196 MPa
28400 psi
ASTM D695