Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fine Organics FINALUX G 211 Lubricant Additive

Category Fluid , Lubricant , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Fine Organics
Trade Name FINALUX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fine Organics FINALUX G 211 Lubricant Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: External lubricants for rigid and soft PVC, specially for Ba-Cd stabilized PVC products.Information provided by Fine Organics
Physical Properties Metric English Comments
Additive Loading 0.20 - 0.50 %
0.20 - 0.50 %
P PVC
0.20 - 0.50 %
0.20 - 0.50 %
R PVC
Thermal Properties Metric English Comments
Melting Point 70.0 - 80.0 °C
158 - 176 °F
Descriptive Properties Value Comments
Influence on Transparency Clear
Lubricating Effect External
Physical Form Solid
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved