Material Notes:
Features: Good drop impact, radiation resistant. Product does not contain animal derived components and is phthalate-free.Applications: Injection MoldingInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 0.942 GPa
137 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Gardner Impact 35.5 J
26.2 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 1.1a and 3.4