Flint Hills 23H2A Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills 23H2A Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent clarity. Product does not contain animal derived components.Applications: Designed for Blow molding and Thermoforming - A replacement for PET, PS and PC high clarity applicationsInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Yield 10.4 %
10.4 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 1130 MPa
164000 psi
ASTM D790
Izod Impact, Notched 2.18 J/cm
4.08 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.6 °C
184 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.2a