Material Notes:
Features: High contact clarity, blush resistant, good impact, and stress resistant, good auto-clave stability, and low extractability. Product does not contain animal derived components.Applications: Suitable for use in food and medical products such as: blow molded containers for irrigation, parenteral, hemodialysis and topical solutionsInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 27.5 MPa
3990 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Tensile Modulus 1.103 GPa
160.0 ksi
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648