Material Notes:
Features: High contact clarity, blush resistant, good impact and flexural modulus. Product does not contain animal derived components.Applications: Blow Molded: Food, health and general purposeInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648