Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Film Grade , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills 44S2A Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Phosphorus free additive package for silicon coated applications. Product does not contain animal derived components.Applications: Extrusion: blown and cast filmInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Tensile Modulus 1.18 GPa
171 ksi
ASTM D638
Flexural Modulus 1.08 GPa
157 ksi
ASTM D790
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648