Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills AP5135-HS Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP5135-HS Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium impact copolymer, FDA compliantFeatures: Nucleated and heat stabilized.Applications: Injection molding: large, thin wall automotive interior parts and housewares.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
23° C; ASTM D256
Gardner Impact 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648