Material Notes:
High impact copolymer, UL certified, and FDA compliant. Features: Nucleated and heat stabilizedApplications: Injection molding: large, thin wall automotive interior parts.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
23° C; ASTM D256
Gardner Impact 27.0 J

@Temperature -30.0 °C
19.9 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648