Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills AP5995-HA Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP5995-HA Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Nucleated with slip, fast cycle times, high flowability.Applications: Injection Molding: High speed packaging applications and thin wall containersInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 100 g/10 min
100 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.5 MPa
3990 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 34.0 J

@Temperature 23.0 °C
25.1 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 1585 MPa
229900 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648