Material Notes:
High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and feed systems for chickens.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Gardner Impact 28.0 J

@Temperature -30.0 °C
20.7 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648