Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Izod Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Gardner Impact 36.0 J

@Temperature 23.0 °C
26.6 ft-lb

@Temperature 73.4 °F
ASTM D5420
36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1069 MPa
155000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Descriptive Properties Value Comments
Instrumented Impact Ductile
6.7 m/s; -30°C; ASTM D3029