Material Notes:
Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.970 GPa
141 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 930 MPa
135000 psi
ASTM D790
Izod Impact, Notched 1.15 J/cm
2.15 ft-lb/in
ASTM D256
Gardner Impact >= 36.2 J
>= 26.7 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a