Flint Hills P5L2K-055 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Blow Molding Grade , Polypropylene, Extrusion Grade
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5L2K-055 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow molding, clear containers and hot fill applications.Information Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.9 g/10 min
1.9 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 1270 MPa
184000 psi
ASTM D790
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 1.00 J

@Temperature -30.0 °C
0.738 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1300 MPa
189000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648