Flint Hills P5M6K-048 Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5M6K-048 Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organoleptic propertiesFormer Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.05 GPa
152 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
23° C; ASTM D256
Gardner Impact 17.0 J
12.5 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ASTM D648